Opinion OF [OOO] “Kuznetsk metal structures”

We express gratitude at the point of the given model of priming enamel “Of [unipol]” OF [SBE]-111 for conducting the tests due to the plant conditions.

The given by you instructions beyond the application of priming enamel “Of [unipol]” OF [SBE]-111, [tekhniologicheskiy] regulations on [primeneni] of priming enamel “Of [unipol]” OF [SBE]-111 (TU 2312-001-3610404-2002) made it possible to conduct tests before several models based on different by surface preparation: the surface of metal with the tightly coupled rust, the rusty surface, [otdrobestruennaya] [poverkhnosti].

As a result carried out tests they revealed:

  1. Adhesion - 1 mark, according to ALL-UNION STATE STAN. 15140-78;
  2. Time of drying - 2 hours according to ALL-UNION STATE STAN. 19007-73;
  3. Relative viscosity - 50 s., according to ALL-UNION STATE STAN. 8420-74.

The results of tests confirm the information, which is contained technological regulations.

Before further work we will propose to planning organizations to include recommendations up the protection of metal structures from the corrosion priming enamel “Of [unipol]” OF [SBE]-111.

With the respect, the director OF [OOO] “KM” Of [sigedin] [I].[A].


© 2004-2005 privately held company “[NPO] Of [korrZashchita]”. All rights are protected. Conditions of using the information

The Russian Federation, 105066, Moscow, ul old [Basmannaya] [d].36.
Bodies: +7 (095) 780-66-09, bodies and the fax: +7 (095) 265-66-09.[Obratnaya] connection
Home Sitemap Contact us

Trusted site that we recommend to visit are:
house rental , fashion blog , used cars , Bathroom Vanities , marchesa , POKEMON